Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 1400 ppm | 1400 ppm | |
ExxonMobil NTX™ NTX 095 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Slip Level | 1400 ppm | 1400 ppm | |
ExxonMobil NTX™ NTX 141 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Slip Level | 1400 ppm | 1400 ppm | |
Bapolene® 142F Polyethylene Film Grade Bapolene 142F is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |