Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |