Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 300000 - 900000 g/mol | 300000 - 900000 g/mol | |
Lucite International Colacryl ® B611 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |
|||
Molecular Weight | 300000 - 900000 g/mol | 300000 - 900000 g/mol | |
Lucite International Colacryl ® B866 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based homopolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.. |
|||
Molecular Weight | 300000 - 900000 g/mol | 300000 - 900000 g/mol | |
Lucite International Colacryl ® D1-120 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |
|||
Molecular Weight | 300000 - 900000 g/mol | 300000 - 900000 g/mol | |
Lucite International Colacryl ® TS2027 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |