Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 900 g/mol | 900 g/mol | |
Dow TONE™ 0310 Polyol TONE™ 0310 polyol is a very low melting tri-functional liquid polyol for use in polyurethane elastomers, coatings, adhesives and soft foams.Information provided by Dow |