Polymer Property : Molecular Weight = 83.98 g/mol
Polymer Property :
Molecular Weight =
83.98 g/mol
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Molecular Weight
83.98
g/mol
83.98
g/mol
MV Labs AL500 AlF3 Aluminum fluoride, anhydrous
Information provided by MV Laboratories.