Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 805 g/mol | 805 g/mol | |
Esstech X-743-0000 Ethoxylated Bis Phenol A Dimethacrylate, C43H64O14 This form of EBPADMA has 10 units of ethoxylation. Polymerization of this material results in a rigid polymer with high degree of conversion. Listed on the Toxic Substance Control Act List. CAS # .. |