Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 8.00e+6 g/mol | 8.00e+6 g/mol | Braskem |
Braskem UTEC® 6540 Ultra High Molecular Weight Polyethylene Applications which require highest wear resistance - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.Information provided by Braskem. |
|||
Molecular Weight | 8.00e+6 g/mol | 8.00e+6 g/mol | Braskem |
Braskem UTEC® 6541 Ultra High Molecular Weight Polyethylene Applications which require highest wear resistance and the use of pigments and/or additives - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.Information provided b.. |