Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 750 g/mol | 750 g/mol | average |
Solvay Specialty Polymers Galden® D02TS PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Molecular Weight | 750 g/mol | 750 g/mol | Mn; ETM E-83 |
ExxonMobil ESCOREZ™ 1102RM (Europe) Petroleum Hydrocarbon Resin Aliphatic hydrocarbon resin specifically designed as a binder for thermoplastic road marking formulations. Availability: Africa & Middle East and EuropeInformation provided by ExxonMobil Chemical |