Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 70.94 g/mol | 70.94 g/mol | |
MV Labs MN800 MnO Manganese(II) oxide Information provided by MV Laboratories. |
|||
Molecular Weight | 70.94 g/mol | 70.94 g/mol | |
American Elements Manganese Oxide Nanopowder General DescriptionManganese Oxide Nanopowder (MnO), nanodots or nanoparticles are high surface area particles. Nanoscale Manganese Oxide Nanoparticles are typically 5 - 100 nanometers (nm) with spe.. |