Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 674.608 g/mol | 674.608 g/mol | |
Esstech X-829-0050 Adhesive Monomer PMGDM, 50% (w/w) Solution in Acetone, C32H34O16 Pyromellitic glycerol dimethacrylate or PMGDM is an excellent liquid adhesive system. Applications exist in both the dental and cosmetic industry. Its' four methacrylate groups help to incorporate i.. |
|||
Molecular Weight | 674.608 g/mol | 674.608 g/mol | |
Esstech X-829-7100 PMGDM, 50% (w/w) Solution in Triethyleneglycol Dimethacrylate, C32H34O16 Dissolving pyromellitic glycerol dimethacrylate or PMGDM in triethyleneglycol dimethacrylate rather than acetone decreases the polarity and odor of this system. The low volatility of TEGDMA also ext.. |