Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 650000 - 850000 g/mol
650000 - 850000 g/mol
Lucite International Colacryl ® TS2050 Acrylic Resin
Lucite® Colacryl® TS2050 is a hard, methyl methacrylate based, acrylic resin with an especially tight particle size distribution, leading to extremely good performance in glass separation appl..