Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 646 g/mol | 646 g/mol | |
Suqian Unitechem Antioxidant 168 Chemical Name: Tris-(2,4-di-tert-butyl-phenyl)-phosphiteCAS NO.: 31570-04-4Molecular Formula: C42H63O3PProperties: The product takes on an appearance of white powder, without odor and smell. Solubl.. |