Physical Properties Metric English Comments
Molecular Weight 625 - 675 g/mol
625 - 675 g/mol
8444
BASF PolyTHF® 650 Polyether
Description: PolyTHF 650 is a colorless, odorless waxy substance. It is sparingly soluble in water and soluble organic solvents.Applications: Intermediate used in the production of: Synthesis of ela..