Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 6200 g/mol | 6200 g/mol | |
Westlake Epolene® N-34 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-34 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Molecular Weight | 6200 g/mol | 6200 g/mol | |
Westlake Epolene® N-34P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-34P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |