Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 6100 g/mol | 6100 g/mol | |
Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water.. |