Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 5.00e+8 - 6.30e+8 g/mol | 5.00e+8 - 6.30e+8 g/mol | |
Silikony Polskie Polimer MV 1.0 Methylvinylsilicone Gum POLIMER MV is the main starting material for production of HTV silicone rubber. Methylvinylsilicone gum should be compounded with crosslinking agents (peroxides), fillers and other additives. Methyl.. |