Polymer Property : Molecular Weight = 591 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 591 g/mol
591 g/mol
Theoretical
PolyOne Synplast™ 810TM-E Tri (n-octyl, n-decyl) Trimellitate
Linear C8-C10 trimellitate ester with antioxidantContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne