Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 58.69 g/mol | 58.69 g/mol | |
American Elements Nickel Nanoparticles General DescriptionNickel (Ni) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Nickel Particles are typically 10 - 40 nanometers (nm) with specific s.. |