Polymer Property : Molecular Weight = 553 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 553 g/mol
553 g/mol
Oceanchem Group Antioxidant 1024
Molecular Formula: C34H52N2O4Uses: Dosage is 0.1-0.5 portions. It is a metal deactivator, can work with antioxidant, used in PE, PP, polystyrene, polyamnamee, polyester, or used as antioxidant of b..