Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 540.46 g/mol | 540.46 g/mol | |
Reade Advanced Materials Montmorillonite - Smectite ((Na,Ca)(Al,Mg)6(Si4O10)3(OH)6-nH2O) Description: A clay mineral having a 2:1 expanding crystal lattice. Isomorphous substitution gives the various types and causes a net permanent charge balanced by cations in such a manner that water.. |