Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 54.94 g/mol | 54.94 g/mol | |
American Elements Manganese Nanoparticles General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 na.. |