Polymer Property : Molecular Weight = 530.87 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 530.87 g/mol
530.87 g/mol
Oceanchem Group Antioxidant 1076
Molecular Formula: C35H62O3Cas No.: 2082-79-3Property: This product is a nonpolluting nontoxic antioxidant with good heat-resisting and water-extracting performance.Characteristics and Uses: This pr..
Molecular Weight 530.87 g/mol
530.87 g/mol
Suqian Unitechem Antioxidant 1076
Chemical Name: Otadecyl Beta-(3,5-di-tert-butyl-4-hydroxyphenyl) propionateCAS NO.: 2082-79-3Molecular Formula: C35H62O3Properties: Soluble in benzene, acetone, hexane, etc, sparingly soluble in met..