Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 521 g/mol | 521 g/mol | |
3M Fluorinert™ FC-3283 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3283 is a non-conductive, thermally and chemically stable liquid ideal for use in single phase heat transfer applications, especially in the electronics and semiconductor.. |