Polymer Property : Molecular Weight = 458 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 458 g/mol
458 g/mol
Average value: 458 g/mol Grade Count:21
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..