Polymer Property : Molecular Weight = 4500 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 4500 g/mol
4500 g/mol
Solvay Specialty Polymers FOMBLIN® W150 PFPE Lubricant
Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc.
Molecular Weight 4500 g/mol
4500 g/mol
BASF Pluracol® 628 Specialty Polyol
Description: Pluracol® 628 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 628 can also be used ..
Molecular Weight 4500 g/mol
4500 g/mol
BASF Pluracol® TP 4542 Specialty Polyol
Description: Pluracol® TPE 4542 polyol is a moderately high molecular weight polyether triol that can be used in polyurethane sealant applications, flexible integral skin foam and cold-cured foam a..