Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 40000 g/mol | 40000 g/mol | |
Lucite International Elvacite ® 4402 Acrylic Resin Elvacite® 4402 is a solid methyl methacrylate copolymer bead resin designed for use in formulating environmentally sound thermosetting coatings and adhesives. The resin may be used as the main b.. |
|||
Molecular Weight | >= 40000 g/mol | >= 40000 g/mol | |
Sichuan Deyang Haton® hb DL Polyphenylene Sulfide Resin Extrusion, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Molecular Weight | >= 40000 g/mol | >= 40000 g/mol | |
Sichuan Deyang Haton® hb Polyphenylene Sulfide Resin Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |