Polymer Property : Molecular Weight = 4.00e+6 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight >= 4.00e+6 g/mol
>= 4.00e+6 g/mol
Polikim ULPOLEN® 1000 UHMWPE Standard
Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia..