Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 399 g/mol | 399 g/mol | |
3M Fluorinert™ FC-770 Electronic Liquid 3M™ Fluorinert™ Liquid FC-770 is a non-conductive, thermally and chemically stable fluid with a wide liquid range (-125 to 95 deg C) for use in many low temperature heat transfer application such .. |