Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 357 g/mol | 357 g/mol | |
Solvay SIPOMER® WAM Allyl / Ureido Monomer Description: Specialty monomer for Wet Adhesion PromotionIdentification: ALLYL / UREIDO MONOMERCAS: 90412 – 00 – 3EINECS: 291 – 480 – 2Solubility: Soluble in water. Insoluble in .. |