Physical Properties Metric English Comments
Molecular Weight 348.8 g/mol
348.8 g/mol
American Elements Samarium Oxide Nanopowder
General DescriptionSM-MITE powders and dispersions are inorganic samarium-oxide nanoparticles. SM-MITE-A products are uncoated and hydrophilic. SM-MITE-O products are coated with an organic silane (..