Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 338.4 g/mol | 338.4 g/mol | |
Esstech X-947-7424 Trimethylolpropane Trimethacrylate, C18H26O6 Trimethylolpropane trimethacrylate or TMPTMA is a unique trifunctional monomer because of its low volatility and its fast cure response. It is also chemical and wear resistant making it ideal for va.. |
|||
Molecular Weight | 338.4 g/mol | 338.4 g/mol | |
Esstech X-947-7446 Trimethylolpropane Trimethacrylate, C18H26O6 Trimethylolpropane trimethacrylate or TMPTMA is a unique trifunctional monomer because of its low volatility and its fast cure response. It is also chemical and wear resistant making it ideal for va.. |
|||
Molecular Weight | 338.4 g/mol | 338.4 g/mol | |
Esstech X-947-7466 Trimethylolpropane Trimethacrylate, C18H26O6 Trimethylolpropane trimethacrylate or TMPTMA is a unique trifunctional monomer because of its low volatility and its fast cure response. It is also chemical and wear resistant making it ideal for va.. |