Physical Properties Metric English Comments
Molecular Weight 336.48 g/mol
336.48 g/mol
MV Labs ND800 Nd2O3 Neodymium oxide
Information provided by MV Laboratories.
Molecular Weight 336.48 g/mol
336.48 g/mol
MV Labs ND810 Nd2O3 Neodymium oxide
Information provided by MV Laboratories.
Molecular Weight 336.48 g/mol
336.48 g/mol
American Elements Neodymium Oxide Nanopowder
General DescriptionND-MITE powders and dispersions are inorganic neodymium-oxide nanoparticles. ND-MITE-A products are uncoated and hydrophilic. ND-MITE-O products are coated with an organic silane ..