Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 329.328 g/mol | 329.328 g/mol | |
Esstech X-863-0050 Surface Active Monomer, NTG-GMA, Sodium Salt, C16H20NO5Na The Sodium Salt of NTG-GMA is an adhesive that bridges the gap between hydrophobic and hydrophilic substrates. It has been traditionally used in dental adhesives. Na Salt of NTG-GMA is TSCA listed a.. |
|||
Molecular Weight | 329.328 g/mol | 329.328 g/mol | |
Esstech X-863-0070 Surface Active Monomer, NTG-GMA, Magnesium Salt, C32H40N2O10Mg The Magnesium Salt of this surface active monomer (NTG-GMA) has similar adhesive characteristics to the sodium salt of NTG-GMA along with improved color. Its' functions are enhanced by an additional.. |