Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 32500 g/mol | 32500 g/mol | |
Lucite International Elvacite ® 4026 Acrylic Resin Elvacite® 4026 is a solid acrylic bead resin which has been specially developed for use as a performance enhancing additive in a range of radiation (UV and EB) curable inks and coatings. These en.. |