Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 291.94 g/mol | 291.94 g/mol | |
Indium Corp. 4N Indium Acetate Indium Acetate is a white powder. It is freely soluble in mineral acid and acetic acid, and exhibits an acetic smell. Its particles are needle-shaped and it decomposes to indium oxide upon heating.. |
|||
Molecular Weight | 291.94 g/mol | 291.94 g/mol | |
Indium Corp. 5N Indium Acetate Indium Acetate is a white powder. It is freely soluble in mineral acid and acetic acid, and exhibits an acetic smell. Its particles are needle-shaped and it decomposes to indium oxide upon heating.. |