Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 26000 g/mol
26000 g/mol
Westlake Epolene® C-16 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified
Product Description: Epolene C-16 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and..
Molecular Weight 26000 g/mol
26000 g/mol
Westlake Epolene® C-16P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-16P is a branched low density polyethylene powder modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and..