Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 254.326 g/mol | 254.326 g/mol | |
Esstech X-887-7424 1,6-Hexanediol Dimethacrylate, C14H22O4 1, 6 - Hexanediol dimethacrylate or HDDMA is a hydrophobic dimethacrylate. It assists with cross-linking and can be used in sealants, adhesives, inks and electronic photopolymers. Listed on the Tox.. |
|||
Molecular Weight | 254.326 g/mol | 254.326 g/mol | |
Esstech X-887-7446 1,6-Hexanediol Dimethacrylate, C14H22O4 1, 6 - Hexanediol dimethacrylate or HDDMA is a hydrophobic dimethacrylate. It assists with cross-linking and can be used in sealants, adhesives, inks and electronic photopolymers. Listed on the Tox.. |
|||
Molecular Weight | 254.326 g/mol | 254.326 g/mol | |
Esstech X-887-7466 1,6-Hexanediol Dimethacrylate, C14H22O4 1, 6 - Hexanediol dimethacrylate or HDDMA is a hydrophobic dimethacrylate. It assists with cross-linking and can be used in sealants, adhesives, inks and electronic photopolymers. Listed on the Tox.. |