Polymer Property : Molecular Weight = 234.77 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 234.77 g/mol
234.77 g/mol
MV Labs AG600 AgI Silver iodide