Physical Properties Metric English Comments
Molecular Weight 222.328 g/mol
222.328 g/mol
Esstech X-724-0000 Isobornyl Methacrylate, C14H22O2
The cyclic group of isobornyl methacrylate allows it to react in free radical polymerization while also acting as an excellent diluent. Listed on the Toxic Substance Control Act List. CAS # 7534-9..