Polymer Property : Molecular Weight = 221.37 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 221.37 g/mol
221.37 g/mol
Dow Corning Z-6011 SILANE
Dow Corning® Z-6011 Silane is a reactive chemical containing an aminopropyl organic group and a triethoxysilyl inorganic group. Chemically, Dow Corning® Z-6011 Silane is designated gammaaminopropy..