Molecular Weight 1950 - 2050 g/mol
1950 - 2050 g/mol
8892
BASF PolyTHF® 2000 Polyether
Description: PolyTHF 2000 is a colorless, odorless waxy substance. It is sparingly soluble in water and soluble organic solvents.Applications: Intermediate used in the production of: Synthesis of el..