Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 201.3 g/mol | 201.3 g/mol | |
Suqian Unitechem Light Stabilizer 201 Product Name: Hydroxyethyl Piperidinol (HS-201)Chemical Name: 1-(2'hydroxyethyl)-2,2,6,6-Tetramethyl-4-piperidinolCAS NO.: 52722-86-8Molecular Formula: C11H23NO2Application: Tetramethyl piperidinol .. |