Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 200000 g/mol
200000 g/mol
Gel Permeation Chromatography
Zeon Chemicals Quintac® 3421 SIS Block Polymer
Styrene Isoprene (SIS) Block Polymer. Standard grade for hot melt PSAInformation provided by Zeon Chemicals L.P.
Molecular Weight 200000 g/mol
200000 g/mol
Gel Permeation Chromatography
Zeon Chemicals Quintac® 3520 SIS Block Polymer
Styrene Isoprene (SIS) Block Polymer. Special grade for PSA (to give high carton sealability)Information provided by Zeon Chemicals L.P.
Molecular Weight 200000 g/mol
200000 g/mol
Gel Permeation Chromatography
Zeon Chemicals Quintac® 3450 SIS Block Polymer
Styrene Isoprene (SIS) Block Polymer. Suitable for HMAInformation provided by Zeon Chemicals L.P.