Physical Properties Metric English Comments
Molecular Weight 2.00e+6 g/mol
2.00e+6 g/mol
Lucite International Lucite® 1192 Glass Separation Resin
Lucite® 1192 is an ultra-high molecular weight PMMA resin, aimed at the protection of hard (metal oxide) coated glass sheets during storage and transportationLucite® 1192 acrylic resin provide..