Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 196 g/mol | 196 g/mol | |
Dow Corning Z-6062 SILANE Dow Corning® Z-6062 Silane is an organofunctional reactive silane. It has a mercaptopropyl and organic group.Information provided by Dow Corning |