Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 19000 g/mol | 19000 g/mol | |
Lucite International Elvacite ® 2927 Acrylic Resin Lucite International has developed novel polymer chemistry which delivers Elvacite® thermoplastic acrylic resins with controlled molecular architecture and enables the coatings formulator to achi.. |