Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 1900 g/mol | 1900 g/mol | Mw; ETM 300-83 |
ExxonMobil ESCOREZ™ 1310 LC Petroleum Hydrocarbon Resin This product is a light colored, premium aliphatic hydrocarbon resin with narrow molecular weight distribution. It is designed to tackify a variety of adhesive polymers including EVA, metallocene .. |