Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 172.12 g/mol | 172.12 g/mol | |
MV Labs CE8005 CeO2 Cerium(IV) oxide Information provided by MV Laboratories. |
|||
Molecular Weight | 172.12 g/mol | 172.12 g/mol | |
American Elements C-MITE™ Cerium Oxide Nanopowder General DescriptionApplicationsC-MITE™ powders and dispersions recently developed are inorganic cerium-oxide nanoparticles with unique polishing and Ultra-Violet attenuating properties. C-MITE-A™ .. |