Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 171.3 g/mol | 171.3 g/mol | |
Suqian Unitechem 1,2,2,6,6-Pentamethyl-4-piperidinol Chemical Name: 1,2,2,6,6-Pentamethyl-4-piperidinolCAS NO.: 2403-89-6Molecular Formula: C10H21NOUses: It is an important intermediate of hindered amine light stabilizer and synthetic hindered amine l.. |