Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 164 g/mol | 164 g/mol | |
Dow Corning TORAY Z-6265 SILANE Propyltrimethoxysilane (C3H7-Si(OCH3)3) High Purity - Hydrophobing & dispersing agent.Information provided by Dow Corning |
|||
Molecular Weight | 164 g/mol | 164 g/mol | |
Dow Corning Z-6264 SILANE Dow Corning® Z-6264 Silane is an alkylalkoxysilane. It has an n-propyl organic group and a trimethoxysilyl inorganic group.Information provided by Dow Corning |